logo

Automatic Four-Head Welding Line For Seismic Bracing Struts

Basic Information
Place of Origin : Guangdong , China
Brand Name : PDKJ
Certification : CE ISO SGS
Model Number : Custom
Trade Information
Minimum Order Quantity : 1 unit
Price : 10000-30000 USD
Standard Packaging : Plywood case
Delivery Time : 15-30 work days
Supply Ability : 100 set per month
Product Summary

Automatic welding line for seismic bracing struts: servo clamp conveyor, pin re-location in the slotted hole, two power sources and four heads in pairs, 30 welds on a 3 m bracket in 150 s.

Product Description
Contents

A 3 m Seismic Bracket Is 30 Spot Welds. Weld One Into The Slotted Hole And You Scrap The Bracket, Not The Weld.

Application story  ·  AZDB-180S dual-power, four-head MFDC welding line for seismic bracing struts - servo-clamped roller conveyor, pin re-location in the slotted hole, 150 s for 30 welds on a 3,048 mm bracket

A seismic bracing strut is a roll-formed C-channel with a row of slotted holes down the web, and the cross members are spot-welded to it at a fixed pitch. The two features fight each other. The slots are punched before the strip is formed, so every hole carries its own tolerance and the error accumulates along the length; the welds, meanwhile, have to land on the flat between the slots. On a 3 m bracket that is thirty chances to put a nugget where a hole is - and a bracket welded into a slot is not re-worked, it is scrapped, because the slot is an anchor point on a services frame and it either takes a fixing or it does not.

Automatic Four-Head Welding Line For Seismic Bracing Struts 

Two-station bracing strut welding line: roller frame and servo clamp carriage along the top of the base, four-head welding units on gantries, exchangeable control pendant on a swing arm

Thirty Welds, Fifteen Strokes, Two Heads Taking Turns

The line is built around two power sources and four welding heads, working in pairs. A 3,048 mm bracket carries 30 welds; two heads at a time makes 15 strokes, and the bracket comes off in 150 seconds. The saving is not only in the stroke count. The part is clamped once, in the servo carriage, and is never handled between welds - which is exactly where a long part picks up the misalignment that makes the welds at the far end wander.

The figure quoted for this line is +80 % per shift against the method it replaced, and the mechanism behind it is the same one an operator would describe: nobody walks the bracket down a bench any more, and nobody re-sets a stop 30 times. The heads also alternate, so neither transformer is asked to dump thirty welds' worth of heat back to back, and the copper stays cooler than a single head doing the same count.

Automatic Four-Head Welding Line For Seismic Bracing Struts 

Roller track and clamp carriages: the two green start buttons and the red stop on the front rail are the operator's whole interface with the cycle

The Slots Are Punched. The Error Adds Up. The Pin Stops It.

The bracket travels on a servo-driven clamp carriage. When it reaches position a pin drops into one of the slotted holes and locates the part a second time. That single action is the argument of the whole machine: the pin does not trust the accumulated position of the slot pattern - it uses the slot in front of it as the datum for the welds in that window. Hole-to-hole tolerance no longer stacks from the head of the bracket to the tail, so the weld pattern stays on the flat at 3 m and at 6 m alike.

Read that as scrap prevention rather than as a precision claim. A weld placed where the slot is cannot be dressed out - the material is gone and the fixing has nothing to bear on. A pin that re-datums every window converts a cumulative error into a local one, and a local error is small enough for the flat between slots to absorb. The same logic is why the carriage grips the part rather than pushing it: a 6 m channel pushed from one end buckles and springs, and a gripped part does not.

Automatic Four-Head Welding Line For Seismic Bracing Struts 

Automatic Four-Head Welding Line For Seismic Bracing Struts 

Automatic Four-Head Welding Line For Seismic Bracing Struts 

Slotted holes and welds on the same web - the weld has to miss the hole

Two sections side by side, one hole pattern each

Detail: weld nuggets between consecutive slots

275 g Of Zinc On The Surface, And An Electrode That Has To Let Go

The struts are hot-dip galvanized at 275 g/m2. Zinc is what makes a spot weld on this part harder than the drawing suggests: at welding temperature it alloys with the copper face of the tip, and the tip starts to pick up. Every stuck tip is a stopped line and a dressing job, and the count of those stops is what a production manager actually experiences as weld quality. The heads here run alumina-copper electrodes, quoted at +70 % resistance to pick-up against a standard tip on this coating.

The electrode is also managed as a consumable with a rule rather than a habit: one dressing per 30 welds, and a tip is retired after 90 dressings. That makes two numbers plannable - how many tips a month of production eats, and how much dressing time sits inside the standard cycle. The head is pre-drilled for an automatic dressing unit, so the rule can later be executed by a device instead of by an operator with a file.

Automatic Four-Head Welding Line For Seismic Bracing Struts 

Four electrodes in a comb on a common secondary: each one slides along the busbar by hand to match the weld pitch, down to 80 mm centre-to-centre

33.4 kN Pull, 66.7 kN Shear - Checked In Four Places

The acceptance figures for the joint are 33.4 kN minimum in pull and 66.7 kN minimum in shear. On a 6,096 mm bracket the check is deliberately not one weld: samples are pulled at the head, four along the middle and at the tail - four segments over the full length - because the question on a long part is never whether the machine can make a good weld. It is whether it makes the same weld at 5.8 m as it does at 0.2 m.

The basis for that consistency is the power source. Medium-frequency DC output is flat, and weld time can be as short as 1 ms, so the heat is delivered into the interface and the heat-affected zone stays small. On 275 g zinc that matters twice over: less coating is boiled out of the joint, and the nugget forms before the zinc has time to alloy with the face of the tip. The weld also comes out flat and tidy, which on a coated strut is not vanity - a burned patch is a visible reject at hand-over.

Automatic Four-Head Welding Line For Seismic Bracing Struts 

Automatic Four-Head Welding Line For Seismic Bracing Struts 

Finished bracket: cross members welded at a fixed pitch along the channel

The strut in service: bolted joints and slotted holes are what the welds must not disturb

80 mm Is The Smallest Pitch. Two Sections, One Line.

The four heads sit in a comb on a common secondary and each slides along the busbar by hand, down to 80 mm centre-to-centre minimum. That is the mechanism behind changing over without changing machines: the two sections in the family, 41 x 41 and 41 x 21, run on the same line once the heads are moved and the programme is called up. A new bracket size is a spacing setting and a weld schedule, not a purchase order.

Capacity growth is handled the same way, electrically. Phase one is two machines discharging alternately, so the peak draw on the plant transformer is that of one machine plus margin rather than of two, and the number of electrodes firing in a cycle can be trimmed further. When the second phase is added the machines are paralleled into the same staggered scheme - more output, no substation upgrade, no renegotiated power contract.

Automatic Four-Head Welding Line For Seismic Bracing Struts 

Two welding units side by side: platen, cylinder stack and air receiver on top, water manifold and filter-regulator on the base

Forty-Five Working Days, And A Technical Agreement Before Either Machine

The line was specified against four problems taken one at a time: matching the electrode to a 275 g coating, carrying a 6 m part on a servo without buckling it, removing the accumulated slot error, and staggering the discharge across machines so the plant supply stays inside its limit. The output was a document - a technical agreement that fixes the weld count, the pitch, the sampling positions, the electrode rule and the acceptance forces. Delivery is 45 working days from that signature.

There is a reason to write it first. After commissioning, the argument on a long bracket is almost never about whether the welder works; it is about where weld number twenty-seven was supposed to be. Fixing the pattern on paper, per bracket size, costs an afternoon. Fixing it in a plant costs a week.

Automatic Four-Head Welding Line For Seismic Bracing Struts 

Roll-formed and hot-dip galvanized strut at 275 g/m2: the coating is what the electrode has to survive, and what the weld must not boil away

Technical Data

Item

AZDB-180S bracing strut welding line

Model

AZDB-180S

Welding process

Medium-frequency inverter DC (MFDC) spot welding

Rated capacity

180 x 2 kVA (dual power source)

Maximum short-circuit current

48 kA

Rated primary current

114 A

Maximum welding force

7,000 N (3 cylinders, 80 x 150 mm)

Throat depth

420 mm

Upper / lower platen gap

350 mm minimum

Welding time

10 s per 2 welds

Cooling water flow

15 L/min, closed circuit with flow switch

Working height

800 - 900 mm (adjustable feet)

Air supply

0.6 - 0.8 MPa

Input power

3-phase 5-wire, 380 V +/- 10 %, 50 Hz

Head pitch

80 mm minimum, manual adjustment along the busbar

 

Item

Part and process

Part

Seismic bracing strut, roll-formed C-channel

Sections

41 x 41 mm and 41 x 21 mm

Bracket lengths

3,048 mm and 6,096 mm

Welds per bracket

30 on a 3,048 mm bracket; 15 double-head strokes

Cycle time

150 s per 3,048 mm bracket

Surface

Hot-dip galvanized, 275 g/m2 zinc

Electrode

Alumina copper; dressed every 30 welds, retired after 90 dressings

Joint acceptance

Pull 33.4 kN minimum; shear 66.7 kN minimum

Sampling

6,096 mm brackets: head, four along the middle, tail - four segments

Capacity

+80 % per shift against the method replaced

Control

Touch-screen welding controller, multiple parameter sets; pre-press, press, pre-weld, slope-up, weld I, weld II, multi-pulse, temper, slope-down

Safety / monitoring

Air and water pressure monitored, low pressure stops the cycle with alarm

Delivery

45 working days from signature of the technical agreement

Dimensions, weld count and acceptance forces above belong to this bracket family. Bracket length, section, weld pitch and sampling plan are fixed per part drawing and confirmed on the customer's own struts during run-off.

Where It Fits

•   Seismic bracing struts for MEP services - water, HVAC and fire protection frames

•   Roll-formed C-channels with punched slotted holes and welded cross members

•   Long parts where the weld pattern has to stay aligned over 3 m and 6 m

•   Hot-dip galvanized strip where electrode pick-up is the limiting factor

•   Two or more sections in one family, changed by head spacing and programme

•   Plants where peak demand has to stay inside the existing transformer

Bracket length, section, weld pitch and weld count are quoted per drawing; head spacing and the weld schedule are set for each part.

From Bracket Drawing To Line

01   Bracket drawing and section: 41 x 41 or 41 x 21, length, hole pattern, zinc weight

02   Weld pattern - count, pitch, and the sampling positions for pull and shear

03   Sample welds on your struts: nugget, surface, pull and shear tear-down

04   Head layout, electrode material and dressing interval

05   Line build - frames, roller track, servo clamp carriages, four heads, two power sources

06   Run-off on customer struts across the bracket lengths in the range

07   Crating, shipment, installation and commissioning

08   Operator training, electrode and spare parts, after-sales support

Talk to Pudian Technology

Guangdong Pudian Automation Technology Co., Ltd builds welding equipment in-house - power sources, controllers, electrodes, fixtures and complete lines - one team, one solution. Welding cross members onto a long punched strut? Send us the bracket drawing and a length of the section, and we will weld a sample bracket and send back the pattern, the pull and shear figures and the tear-down photographs.

Guangdong Pudian Automation Technology Co., Ltd

WhatsApp / Tel: +13613793248    Email: jay@gd-pw.com

Website: https://www.spotlaserwelding.com/

Address: 1-2F, Building 3, Qichen Industrial Park, No. 26 Luxi 1st Road, Liaobu Town, Dongguan City, Guangdong Province, China


Send Us An Inquiry
We will reply to you within 24 hours.
Inquiry Details
Contact Information